Spherical Inconel 718 Superalloy Powder
CAS —
IN718 · 2.4668
AM / 3D-Printing Powder
Powder Characteristics
| Property | Value | Test Method |
| Particle Size Cut | 15–53 μm (other cuts on request) | Laser diffraction |
| PSD, typical (D10/D50/D90) | 16 / 36 / 53 μm | Laser diffraction |
| Flowability (Hall), typical | ≈ 15.5 s/50 g | ASTM B213 / GB-T 1482 |
Typical values per manufacturer COA; lot values may vary. Lot-specific COA & PSD report supplied with each shipment.
Chemical Composition (Specification)
| Element / Component | Specification | Test Method |
| Nickel (Ni) | 50–55% | ICP-OES / LECO |
| Chromium (Cr) | 17–21% | ICP-OES / LECO |
| Niobium (Nb) | 4.75–5.5% | ICP-OES / LECO |
| Molybdenum (Mo) | 2.8–3.3% | ICP-OES / LECO |
| Titanium (Ti) | 0.65–1.15% | ICP-OES / LECO |
| Aluminum (Al) | 0.2–0.8% | ICP-OES / LECO |
| Iron (Fe) | Balance | ICP-OES / LECO |
Typical Applications
- Laser Powder Bed Fusion (LPBF/SLM)
- Directed Energy Deposition (DED)
- Aerospace & gas-turbine components
- High-temperature fasteners & tooling
- Repair cladding
Packaging
Vacuum-sealed argon-filled containers; quantity per inquiry
Storage & Shelf Life
Sealed, dry, inert atmosphere recommended. Avoid moisture.
All values are typical and may vary by lot. This TDS does not constitute a warranty.